Discussion on uneven gloss of plastic mold products


Release time:

2023-02-11

Due to poor distribution of pigments or fillers, the color of plastic or pigment discoloration on the surface of plastic parts is uneven. The reasons for uneven color vary depending on the phenomenon presented. The uneven distribution of pigments near the feeding port is mainly caused by poor thermal stability of the plastic when the color of the entire plastic part is uneven, and the uneven color of the fusion joint is related to the properties of the pigments.

Due to poor distribution of pigments or fillers, the color of plastic or pigment discoloration on the surface of plastic parts is uneven. The reasons for uneven color vary depending on the phenomenon presented. The uneven distribution of pigments near the feeding port is mainly caused by poor thermal stability of the plastic when the color of the entire plastic part is uneven, and the uneven color of the fusion joint is related to the properties of the pigments.

Uneven gloss of plastic mold products:

1. The cooling rate and properties of the rubber material result in different glosses;

2. Uneven gloss may occur in areas where the mold temperature is too low;

3. The temperature of the rubber material is too low;

4. Using excessive release agents;

5. Poor surface polishing of the mold;

Analysis of the reasons for uneven gloss of plastic parts:

1. Aluminum foil or thin sheet pigments have luster along the direction of the material flow, and the pigments have no directional distribution and uneven color at the feeding port, fusion joint area, and multiple feeding ports;

2. Poor pigment quality;

3. When rolling and stirring, the pigment only adheres to the surface of the material particles;

4. Plunger injection molding machines are prone to uneven color;

5. Uneven plasticization;

6. Uneven distribution of fiber fillers, accumulation and exposure, or resin dissolution when plastic parts come into contact with solvents, resulting in exposed fibers;

7. Decomposition of plastics or pigments;

8. There is moisture, oil stains, or excessive release agent on the surface of the mold;

9. Mixing different materials into plastics and pigments;

10. Low crystallinity or uneven wall thickness of plastic parts, affecting transparency and causing uneven color;

Dongguan Qianglian Machinery Casting Co., Ltd. is a wholly-owned Taiwanese enterprise. In 2001, our equipment operation company adheres to the business philosophy of "customers are our life quality is our mission" and "integrity". The products are sold domestically and exported to countries and regions such as Japan, Taiwan, and Europe. The company covers a total area of 50000 square meters, with a factory building area of 30000 square meters.

Production capacity: Annual production capacity 26000 tons, with a maximum casting capacity of 45 tons per piece.

Main products: Mechanical casting, such as automotive molds, punches, machining centers, gantry milling machines, injection molding machines.

Exclusive: nodular cast iron FCD40-70, Gray iron FC25-35, automobile mold GM246241.